Precautions for ceramic kiln firing
Belongs to category: Industry News
Release Time: 2022-11-22
Summary: 1. Cooling the kiln too quickly can cause the porcelain to crack; 2. Insufficient oxidation time and rapid firing can cause blistering; 3. Uneven firing can easily lead to deformation; 4. Uneven kiln temperature and overheating can cause the porcelain to swell; 5. If the firing method and flame properties are not suitable, the porcelain surface may discolor and develop stains;
1. Cooling the kiln too quickly can cause the porcelain to crack;
2. Insufficient oxidation time and rapid kiln firing can cause blistering;
3. Uneven kiln firing can easily lead to deformation;
4. Uneven kiln temperature and overheating can cause the porcelain to swell;
5. If the firing method and flame properties are not suitable, the porcelain surface may discolor and develop stains;
Keywords: Precautions for ceramic kiln firing
Related Information
Industry News
-
News | Guangdong's first natural gas hydrogen-doped ceramic shuttle kiln ignited successfully
Time:2025-05-23
-
Heat transfer characteristics of shuttle kilns
Time:2022-11-22
-
Tunnel kilns have various different classifications
Time:2022-11-22
-
The structural composition of a shuttle kiln
Time:2022-11-22
-
How to choose a ceramic kiln
Time:2022-11-22
-
Matters needing attention when re-igniting the kiln
Time:2022-11-22
-
What are the classifications of ceramic factory kilns?
Time:2022-11-22
-
Burning analysis
Time:2022-11-22
-
Precautions for ceramic kiln firing
Time:2022-11-22
-
Introduction to Wenyao Technology
Time:2022-11-22
-
What is ceramic fiber? What are the uses of ceramic fiber?
Time:2022-11-22
Previous: Burning analysis